Allegheny Ludlum Alloy 825™ Corrosion Resistant Alloy, UNS N08825
Subcategory: Superalloy; Nickel Base
Key Words: DIN 2.4858; ASTM B-424; ASME SB-424
Material Notes: Iron content above calculated as remainder. Available in plate, sheet, and strip. For use in neutral or moderately oxidizing environments. Specific uses incluse pollution control and radioactive waste equipment, chemical transport and acid production equipment, pickling equipment, oil/gas well piping. Information provided by Allegheny Ludlum