Allegheny Ludlum Stainless Steel AL 904L™ Alloy (UNS N08904)
Subcategory: T 400 Series Stainless Steel; Stainless Steel; Metal
Key Words: DIN 1.4539; ASTM B-625; ASME SB-625
Material Notes: Iron content above calculated as balance. Allegheny Ludlum AL 904 L™ Alloy (UNS N08904) is an austenitic stainless steel alloy designed for a middles to high level of corrosion resistance. The alloy is produced to low carbon levels for use in the welded condition as in welded vessels and other large and complex fabrications. The high nickel (25%) and molybdenum (4.5%) contents of the AL 904L alloy provide good resistance to chloride stress corrosion cracking, although not total resistance as judged by the extremely severe laboratory test, boiling magnesium chloride. The N08904 alloy has been incorporated in ASTM and ASME specifications, and is widely and readily available in a variety of product forms, welding electrodes, and fittings. The AL 904L Alloy has performed well in a variety of service environments such as utility scrubbers, acid and fertilizer production. Information provided by Allegheny Ludlum Corporation.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Electrical Resistivity
- Magnetic Permeability
- CTE, linear 20°C
- CTE, linear 500°C
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|