Allegheny Ludlum AL 42™ Electrical Alloy, UNS K94100

 

Subcategory: Electronic/Magnetic Alloy

Key Words: ASTM F-30 (42)

Material Notes:
Iron content above calculated as remainder.

AL 42 alloy is used extensively in the manufacture of sealed beam automobile head lamps, in grommet and pin type glass-metal seals, and in integrated circuit lead frames. It is also the core metal used in the manufacture of Dumet wire. AL 42 alloy has a low expansion coefficient used to match the expansion characteristics of 98% alumina and hard borosilicate glasses. In its various annealed or tempered conditions AL 42 alloy has excellent formability, good stampability, good photoetching characteristics and is solderable. The alloy is fully austenitic at all application temperatures. Where glass-metal sealing is involved, the alloy is usually stabilized with titanium additions to prevent evolution of carbon dioxide bubbles in the glass-metal interface. A titanium stabilized version is available for glass-to-metal seal applications where formation of carbon dioxide bubbles is to be avoided during fabrication.

Information provided by Allegheny Ludlum

Available Properties
  • Density
  • Hardness, Rockwell B
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Electrical Resistivity
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。