Allegheny Ludlum Moly Permalloy Electrical Alloy

 

Subcategory: Electronic/Magnetic Alloy

Key Words: ASTM A-753; MIL-N-14411

Material Notes:
Iron content above calculated as remainder.

An alloy with exceptionally high magnetic permeability, very low coercive force, very low core losses, and low reminance by magnetic field annealing. The alloy finds application in magnetic shielding where fields much less than the Earth's magnetic filed are required. The highest volume applications using laminations or tape wound cores today are ground fault interrupter and modem transformer cores. The alloy is used as well in a variety of other high performance transformer core applications such as tape recorder heads and audio transformers. Control of the cooling rate during heat treatment and superimposition of various customer bake treatments are used to develop the most suitable magnetic quality for the application.

Information provided by Allegheny Ludlum

Available Properties
  • Density
  • Hardness, Rockwell B
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Electrical Resistivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。