Allegheny Ludlum Stainless Steel JS700® Alloy (UNS N08700)
Subcategory: Stainless Steel; Metal
Key Words: ASTM B599, ASTM B672, ASTM SB599, ASTM SB672
Material Notes: Iron content above calculated as balance. Allegheny Ludlum's Corrosion resistant engineering alloy, JS700®, is a high-alloy, fully austenitic, superaustenitic stainless steel. This alloy is a proven problem-solver in many applications where corrosive conditions are too severe for standard grades of stainless steel. It has also provided a cost-effective alternative to more expensive nickel-base and titanium-base alloys. JS700 stainless steel is more highly alloyed than standard stainless steels. The high molybdenum content is particularly important to the corrosion resistant properties. It enhances development of the passive film responsible for the corrosion resistance of stainless, and makes the alloy more noble so that corrosion resistance is improved even under conditions which tend to destroy passivity. The chromium content of the JS700 is essential to corrosion resistance. Since chromium contributes to sigma formation, the 20% level was chosen as a satisfactory compromise. The high nickel content not only minimizes sigma, but also contributes markedly to corrosion resistance. The effects of higher nickel are believed to relate more to corrosion propagation than to initiation. The combination of the three major alloying elements gives JS700 stainless steel a high degree of resistance to stress corrosion cracking. No field service failures from stress corrosion cracking in JS700 Alloy have been reported to date. Information provided by Allegheny Ludlum Corporation.
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- CTE, linear 20°C
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|