Allegheny Ludlum AL 22™ Nickel-Base Alloy, UNS N06022

 

Subcategory: Superalloy; Nickel Base

Key Words: Specs: ASTM B-575; ASME SB-575

Material Notes:
Nickel content above calculated as remainder.

AL 22 alloy is a Ni-Cr-Mo alloy that provides outstanding resistance to pitting, crevice corrosion, intergranular attack, and stress corrosion cracking. The combination of Cr, Ni, Mo, and W provides excellent resistance to a broad range of both oxidizing and reducing environments. Allegheny Ludlum's plate mill has been producing this allow since 1987. The alloy is used in a wide range of applications including flue-gas desulfurization systems, bleaching processes in pulp-and-paper plants, waste incinerators, sour gas service, chemical processing plants, pharmaceutical plants, and radioactive waste storage.

The AL 22 alloy possesses high strength, good ductility, excellent welding and forming characteristics. The alloy has been incorporated in ASTM and ASME specifications and is available in a wide range of product forms such as plate, sheet, strip, tube, pipe, bar, billet, and forgings.

Information provided by Allegheny Ludlum

Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Rockwell B
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • CTE, linear 20°C
  • CTE, linear 250°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。