Allegheny Ludlum Altemp® 718 Nickel-Base Superalloy, Solution Treated Plate, UNS N07718

 

Subcategory: Superalloy; Nickel Base

Key Words: DIN 2.4668; ASTM B-670; AMS 5596; AMS 5597

Material Notes:
Iron content above calculated as remainder.

Allegheny Ludlum Altemp 718 alloy is an austenitic nickel-base superalloy which is used in applications requiring high strength to approximately 760 degrees Celsius and oxidation resistance to approximately 982 degrees Celsius. In addition, the alloy exhibits excellent tensile and impact strength even at cryogenic temperatures. High strength at room and elevated temperatures is developed by a precipitation heat treatment at 718 degrees Celsius with cooling and a hold at 621°C.

The relatively slow response to precipitation hardening permits repair welding of the Altemp 718 alloy even in the aged condition. The Altemp 718 alloy is usually produced by a double melt practice using consumable electrode remelt procedures to provide homogeneity and extremely clean structures. Uses include aircraft ducting and engine plumbing.

Tensile properties below are from AMS 5596 and/or AMS 5597.

Information provided by Allegheny Ludlum

Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Poissons Ratio
  • Shear Modulus
  • Electrical Resistivity
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。