Allegheny Ludlum AL 15-5™ High Strength Stainless Steel, UNS S15500
Subcategory: Stainless Steel; Precipitation Hardening Stainless; Metal
Key Words: DIN 1.4545; ASTM A693; ASME SA693; AMS 5562, 15-5PH, 15-5 PH, 15/5PH, 15/5 PH, Precipitation Hardening
Material Notes: Iron content above calculated as remainder. Property data below is typical of annealed samples. Available in plate. For use in fasteners, military equipment and air frame parts. Information provided by Allegheny Ludlum
| Available Properties |
- Density
- Hardness, Rockwell C
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|
| Property Data |