Allegheny Ludlum AL 17-7™ High Strength Stainless Steel, UNS S17700
Subcategory: Stainless Steel; Precipitation Hardening Stainless; Metal
Key Words: 17-7PH, 17-7 PH, 17/7PH, 17/7 PH, DIN 1.4568; ASTM A-693; ASME SA-693; AMS 5528; AMS 5529 (Cold rolled temper), Precipitation Hardening
Material Notes: Iron content above calculated as remainder. Property data below is typical of annealed samples. Available in sheet and strip. For use in high-strength springs, bellows, and aerospace applications. Information provided by Allegheny Ludlum
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|
| Property Data |