Allegheny Ludlum H13 Tool Steel, UNS T20813
Subcategory: Tool Steel; Hot Work Steel; Metal
Key Words: AMS 6408, ASTM A681(94), FED QQ-T-570(87), SAE J437(70), SAE J438(70), SAE J467(68), BS 4659 BH13, BS 4659 H13, AFNOR NFA35590 Z40CDV5, DIN 17350(80) GX40CrMoV5-1, UNE 36072/2(75) X40CrMoV5
Material Notes: Iron content above calculated as remainder. An excellent hot work grade with an outstanding combination of shock resistance, red hardness, and abrasion resisting properties. Typical application include die casting dies, hot forging dies, hot press dies, dies holder blocks, hot work punches and plastic molding dies. Information provided by Allegheny Ludlum
| Available Properties |
|
We're sorry, but our sources do not report any other information for this material.
|
|
|
|