Allegheny Ludlum Titanium 6Al-4V ELI (UNS R56401)
Subcategory: Titanium Alloy; Nonferrous Metal; Alpha/Beta Titanium Alloy
Key Words: Ti 6-4; Titanium 6-4; ASTM B-265; ASTM F-136; ASME SB-265; AMS 4907-4; MIL-T-9046
Material Notes: Titanium content above calculated as remainder. The ELI grade has lower impurity limits than standard titanium 6-4. Uses: applications requiring excellent fracture toughness and fatigue strength, aircraft, structural components, biomedical. Mechanical property data below is typical of annealed samples at room temperature. Information provided by Allegheny Ludlum.
| Available Properties |
- Density
- Hardness, Rockwell C
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|