Allegheny Ludlum Grade 17 Titanium (UNS R52252)
Subcategory: Titanium Alloy; Nonferrous Metal; Unalloyed/Modified Titanium
Key Words: ASTM B-265
Material Notes: Titanium content above calculated as remainder. Uses: CPI equipment, industrial components, plate frame heat exchangers. Mechanical property data below is typical of annealed samples at room temperature. Information provided by Allegheny Ludlum.
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|