Allegheny Ludlum M3 Tool Steel, UNS T11313
Subcategory: Tool Steel; Metal
Material Notes: Iron content above calculated as remainder. Slightly higher wear resistance and lower toughness than M2. Typical application similar to that of M2. Information provided by Allegheny Ludlum