Lucas-Milhaupt AL 719 Aluminum Brazing Filler Metal

 

Subcategory: Aluminum Alloy; Nonferrous Metal; Solder/Braze Alloy

Material Notes:

Applications:AL 719 filler metal is generally used to join aluminum and aluminum alloys. It has been used to join castings and otherwise unbrazeable aluminums. Care must be taken to be sure that the heat treatment (if any) is compatible with the brazing materials and process. Because of this high alloy content of AL 719, the corrosion resistance is not as good as other aluminum filler metals.

Characteristics:AL 719 is a filler metal for use with brazeable aluminums where a flux process is used. Because of its high zinc content this material is not recommended for vacuum brazing. To prevent liquation, it is recommended that the parts be heated rapidly thru the solidus-liquidus temperature range.

Specifications: AL 719 meets the requirements for the following specifications-Aluminum Association (AA) 4245

Information provided by Lucas-Milhaupt, Inc.

Available Properties
  • Density
  • Specific Gravity
  • Solidus
  • Liquidus
  • Processing Temperature
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。