Lucas-Milhaupt HANDY HI-TEMP 870 High Temperature Alloy

 

Subcategory: Copper Alloy; Nonferrous Metal; Solder/Braze Alloy

Material Notes:

Characteristics:Because of the wide melting range, this filler metal has good gap filling characteristics at the lower end of the brazing range and is relatively free-flowing near the upper end. Wetting is excellent on carbide stainless steel and copper. Recommended brazing clearances are .006"-.012". Fluxless braze in a vacuum or suitable protective atmosphere, or induction or furnace braze using Handy Hi-Temp M, Handy Hi-Temp DB or Handy Hi-Temp Boron Modified Flux.

Applications:Handy Hi-Temp 870 is a bronze filler metal used for tungsten carbide to steel joints or stainless steels, requiring optimum high temperature shear strength, toughness and corrosion resistance. Brazing is often done in conjunction with heat treatment of the steel.

Information provided by Lucas-Milhaupt, Inc.

Available Properties
  • Specific Gravity
  • Density
  • Shear Strength
  • Electrical Resistivity
  • Solidus
  • Liquidus
  • Processing Temperature
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。