Lucas-Milhaupt HANDY HI-TEMP 870 High Temperature Alloy
Subcategory: Copper Alloy; Nonferrous Metal; Solder/Braze Alloy
Material Notes:
Characteristics:Because of the wide melting range, this filler metal has good gap filling characteristics at the lower end of the brazing range and is relatively free-flowing near the upper end. Wetting is excellent on carbide stainless steel and copper. Recommended brazing clearances are .006"-.012". Fluxless braze in a vacuum or suitable protective atmosphere, or induction or furnace braze using Handy Hi-Temp M, Handy Hi-Temp DB or Handy Hi-Temp Boron Modified Flux. Applications:Handy Hi-Temp 870 is a bronze filler metal used for tungsten carbide to steel joints or stainless steels, requiring optimum high temperature shear strength, toughness and corrosion resistance. Brazing is often done in conjunction with heat treatment of the steel. Information provided by Lucas-Milhaupt, Inc.
| Available Properties |
- Specific Gravity
- Density
- Shear Strength
- Electrical Resistivity
- Solidus
- Liquidus
- Processing Temperature
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|