Lucas-Milhaupt BRAZE 051 Silver Based Cadmium Free Filler Metal
Subcategory: Copper Alloy; Zinc Alloy; Nonferrous Metal; Solder/Braze Alloy
Material Notes:
Characteristics:Braze 051 is a low cost, intermediate temperature silver brazing filler metal suitable for joining various ferrous and non-ferrous alloys that can be heated to 1650EF/900EC without damage. The relatively high flow point of this filler metal, combined with its high zinc content, tends to cause a rapid alloying of Braze 051 with non-ferrous alloys. For this reason, the time the brazing alloy is kept molten, in contact with the base metal, should be kept to a minimum. In furnace brazing, the heating cycle should be kept short to avoid excessive volatilization of the zinc with resultant formation of pinholes in the brazing alloy layer. Applications:The high flow point and narrow melting range of Braze 051 are useful for applications where the brazing and heat treating of ferrous alloys are combined in one operation. The alloy is useful for brazing Nichrome resistance wires because the brazing temperature is high enough to cause stress relief annealing of the Nichrome thus avoiding intergranular cracking. Information provided by Lucas-Milhaupt, Inc.
| Available Properties |
- Density
- Specific Gravity
- Electrical Resistivity
- Solidus
- Liquidus
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|