Lucas-Milhaupt BRAZE 450 Silver Based Cadmium Free Filler Metal

 

Subcategory: Silver Alloy; Copper Alloy; Zinc Alloy; Nonferrous Metal; Solder/Braze Alloy

Material Notes:

Characteristics:Braze 450 is an intermediate temperature cadmium free silver brazing filler metal with sufficient melting range (145EF) to properly braze joints with the range of fits encountered in commercial tubing and fittings. It has a slight tendency to liquate (i.e. separate into high and low melting constituents) if heated slowly through its melting range.

Applications:Braze 450 has found considerable application in pipe brazing in the ship construction industry and for such items as band instruments, brass lamps, aircraft engine oil coolers, plus other situations where a high strength, ductile joint is required. It is a good, general purpose, brazing filler metal for use where a cadmium free filler metal is specified.

Specifications:Braze 450 conforms to the following specifications- AWS A5.8 BAg-5, ASME Boiler & Pressure Vessel Code Sec. II C, SFA-5.8 BAg-5

Information provided by Lucas-Milhaupt, Inc.

Available Properties
  • Density
  • Specific Gravity
  • Tensile Strength @ Break
  • Elongation at Break
  • Electrical Resistivity
  • Solidus
  • Liquidus
  • Processing Temperature
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。