Lucas-Milhaupt BRAZE 603 Silver Based Cadmium Free Filler Metal
Subcategory: Silver Alloy; Copper Alloy; Nonferrous Metal; Solder/Braze Alloy
Material Notes:
Characteristics: Braze 604 is a low temperature, low vapor pressure brazing filler metal formulated to meet the need for a composition free from volatile constituents, particularly essential in the brazing of vacuum tubes. The tin content of this filler metal improves its wetting characteristics on ferrous alloys over that obtainable with binary silver-copper filler metals. The tin addition also lowers the melting range versus binary silver-copper compositions. There is some tendency for the filler metal to liquate, but this is minimized by rapid heating to brazing temperature. Applications: Braze 603 is a silver-base brazing metal useful for making low temperature seals on vacuum tube components and for controlled atmosphere brazing of ferrous and non-ferrous alloys without flux. These filler metals are also recommended for brazing marine heat exchangers that are in contact with salt water, where there is a danger of dezincification to alloys containing zinc, particularly with joints on copper-nickel tubing. Specifications:This filler metals conform to the following specifications: AWS A5.8 BAg-18, ASME Boiler and Pressure Vessel Code Section II-C SFA 5.8 Information provided by Lucas-Milhaupt, Inc.
| Available Properties |
- Density
- Specific Gravity
- Electrical Resistivity
- Solidus
- Liquidus
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|