Lucas-Milhaupt BRAZE 716 (VTG) Grade 2 Silver Based Cadmium Free Filler Metal
Subcategory: Silver Alloy; Copper Alloy; Zinc Alloy; Nonferrous Metal; Solder/Braze Alloy
Material Notes:
Characteristics: Braze 716 is a nickel modified silver copper eutectic filler metal. The addition of nickel renders this alloy somewhat more sluggish in flow characteristics than the eutectic composition but improve the wettability on ferrous alloys. On either silver, nickel, or copper base alloys Braze 716 exhibits a decrease in fluidity and an increase in remelt temperature, after brazing, due to the solution of some base metal in the filler metal. Specifications: This filler metal conforms to the following specifications: AMS 4766, AWS A5.8 BVAg-8b, Grade 2 Information provided by Lucas-Milhaupt, Inc.
| Available Properties |
- Density
- Specific Gravity
- Tensile Strength @ Break
- Elongation at Break
- Electrical Resistivity
- Solidus
- Liquidus
- Processing Temperature
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|