Lucas-Milhaupt BRAZE 720 Silver Based Cadmium Free Filler Metal

 

Subcategory: Silver Alloy; Copper Alloy; Nonferrous Metal; Solder/Braze Alloy

Material Notes:

Characteristics:Brazing 720 is the silver-copper eutectic composition and in melting it acts like a metallic element, i.e. it melts completely at a single temperature, thus it will quickly flow into long narrow joints. On either silver base of copper base alloys, Braze 720 exhibits a decreased fluidity and an increased remelt temperature due to the solution of either silver or copper in the eutetic. Brazing time and temperature should be minimized to prevent excessive diffusion and erosion of the base metal.

This filler metal has limited wetting ability on iron and/on nickel base alloys. The wetting ability it does have is derived from its copper content. Both iron and nickel have practically no solubility in silver, while nickel is readily soluble in copper and the solubility of iron in copper is sufficient to provide wetting. It is an observed fact that the wetting obtained in good hydrogen atmospheres is superior to that derived from flux protection.

Applications: Braze 720 is generally used to join silver, copper and nickel base alloys in reducing or inert atmospheres or vacuum. It is also widely used to join metallized ceramics to metals in vacuum.

Specifications: This filler metal conforms to the following specifications: AWS A5.8 BAg-8, ASME Boiler & Pressure Vessel Code, Sec. II-C, SFA 5.8 BAg-8

Information provided by Lucas-Milhaupt, Inc.

Available Properties
  • Density
  • Specific Gravity
  • Tensile Strength @ Break
  • Electrical Resistivity
  • Solidus
  • Liquidus
  • Processing Temperature
  • Color
  • Corrosion Resistance
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。