Lucas-Milhaupt BRAZE 721 (VTG) Grade 1 Silver Based Cadmium Free Filler Metal
Subcategory: Silver Alloy; Copper Alloy; Nonferrous Metal; Solder/Braze Alloy
Material Notes:
Applications: Braze 721, a VTG version of Braze 720, is designed for all types of moderate temperature vacuum systems and particularly where maximum precautions must be taken to insure the presence of only a minimum amount of detrimental volatile impurities. Specifications: This filler metal conforms to the following specifications: AWS A5.8 BVAg-8 Grade 1, ASME Boiler & Pressure Vessel Code, Sec. II-C, SFA 5.8 BAg-8 Information provided by Lucas-Milhaupt, Inc.
| Available Properties |
- Density
- Specific Gravity
- Tensile Strength @ Break
- Electrical Resistivity
- Solidus
- Liquidus
- Processing Temperature
- Color
- Corrosion Resistance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|