Lucas-Milhaupt BRAZE 852 Silver Based Cadmium Free Filler Metal

 

Subcategory: Silver Alloy; Nonferrous Metal; Solder/Braze Alloy

Material Notes:

Characteristics: Braze 852 is a high temperature, free flowing silver brazing filler metal usable both for torch and atmosphere furnace brazing.

Due to the high flow point of this alloy, torch brazing is accomplished with Handy Hi-Temp Flux or Handy Hi-Temp Flux Boron Modified. These fluxes may also be required as a supplement when brazing parts in a controlled atmosphere furnace. Even at 2000EF a dew point of -80EF or better is required to reduce manganese oxides in hydrogen.

Applications: Braze 852 is used principally for applications requiring good strength, at elevated temperatures, in service. This alloy is useful for brazing stainless steels, Stellite and Inconel. It is also effective for brazing certain complex chromium-titanium carbides and is used where carbide tools may encounter high operating emperatures in service. When parts are heat treated subsequent to brazing the high melting point of this alloy is an advantage.

Specifications: This alloy conforms to the following specifications: AMS 4766, AWS A5.8 BAg-23, ASME Boiler and Pressure Vessel Code Section II-C SFA 5.8 BAg-23

Information provided by Lucas-Milhaupt, Inc.

Available Properties
  • Density
  • Specific Gravity
  • Tensile Strength @ Break
  • Tensile Strength, Ultimate at Elevated Temperature
  • Electrical Resistivity
  • Solidus
  • Liquidus
  • Processing Temperature
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。