Lucas-Milhaupt Lithobraze 925 Silver Based Cadmium Free Filler Metal

 

Subcategory: Silver Alloy; Nonferrous Metal; Solder/Braze Alloy

Material Notes:

Applications: The principal use to date of Lithobraze 925 has been the brazing of honeycomb panel sections. It can be used for general purpose furnace brazing of stainless steels where flux must be avoided.

Characteristics: Lithobraze 925 is lithium modified sterling silver, designed primarily for fluxless furnace brazing of stainless steels. This alloy has been widely used for brazing honeycomb airframe structures made of precipitation hardening stainless steels such as 17-7PH, PH15-7Mo and AM350.

The use of Lithobraze 925 permits taking advantage of the maximum panel strength afforded by free node flow. This alloy is not suitable for torch brazing in air but must be used in a hydrogen or inert atmosphere of low dew point (-70EF/-55EC or drier). Argon is the most commonly used inert gas.

Information provided by Lucas-Milhaupt, Inc.

Available Properties
  • Density
  • Specific Gravity
  • Electrical Resistivity
  • Solidus
  • Liquidus
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。