Lucas-Milhaupt Premabraze 616 Silver Based Cadmium Free Filler Metal

 

Subcategory: Silver Alloy; Indium Alloy; Nonferrous Metal; Solder/Braze Alloy

Material Notes:

Applications: Application is found in all types of moderate temperature low pressure systems, and in particular the electronic vacuum tube.

Characteristics:Premabraze 616 is a low temperature, slightly sluggish brazing filler metal with a tendency to liquate (i.e. separate into low and high melting constituents) if heated slowly through their melting range. This low vapor pressure brazing filler metal was formulated to meet the need for a composition free from volatile constituents, particularly in the brazing of vacuum tubes. This filler metal can be successfully used in hydrogen, inert atmospheres or vacuum without flux. The indium content improves their wetting tendency on ferrous alloys over that obtainable with binary silver-copper.

Some nickel base alloys are susceptible to stress cracking. To prevent this the parts should be stress-relieved prior to brazing. Special attention should also be given to dissimilar metal joints where stresses can occur from differences in thermal expansion.

Specifications:Premabraze 616 conforms to AWS A5-8, BVAg-29, Grade 2.

Information provided by Lucas-Milhaupt, Inc.

Available Properties
  • Specific Gravity
  • Electrical Resistivity
  • Solidus
  • Liquidus
  • Processing Temperature
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。