Lucas-Milhaupt BRAZE 053 (TEC) Silver Based Cadmium-Bearing Filler Metal

 

Subcategory: Silver Alloy; Nonferrous Metal; Solder/Braze Alloy

Material Notes:

Applications: This solder has been used where alloys melting higher than soft solders are required but the strength of standard solder brazing filler metals is not necessary. An example of this is the use in thermostatic bellows where the operating temperature is too high for soft solders and the bellows must be joined below their annealing temperature.

A large use has been on small electric motors for soldering copper leads which would fail on overheating if soft soldered.

Another use has been in soldering gun parts, replacing soft solders, In this case the advantages are strength at higher temperatures than soft solders can withstand and an increase in the corrosion resistance to alkaline solutions used in blackening gun barrels.

Because of the high cadmium content of the filler metal, it should not be used for joining food containers.

Characteristics: The flow point of Braze 503 is intermediate between soft solders and standard silver brazing filler metals. As a result, a special flux-Handy Flux Type TEC (a liquid flux) - has been developed for use with this filler metal, because the active temperature range of soft solder fluxes is too low while that of the silver brazing fluxes is too high.

Braze 053, when used with Handy Flux Type TEC, will join such metals as copper, brass and steels.

Information provided by Lucas-Milhaupt, Inc.

Available Properties
  • Density
  • Specific Gravity
  • Electrical Resistivity
  • Solidus
  • Liquidus
  • Processing Temperature
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。