Lucas-Milhaupt SIL-FOS 18 Silver/ Copper/ Phosphorus Alloy

 

Subcategory: Silver Alloy; Copper Alloy; Nonferrous Metal; Solder/Braze Alloy

Material Notes:

Applications: Sil-Fos 18 is a moderate cost brazing filler metal suitable for joining copper, brass and bronze alloys where low brazing temperature and free flowing characteristics are required. It should be used on assemblies where good fitup can be maintained.

Characteristics: Sil-Fos 18 is a ternary eutectic, low temperature brazing filler metal that is free flowing and self-fluxing on copper and some high copper an copper alloys by virtue of its phosphorus content. Brasses and most bronzes require the use of Handy Flux (or Handy Flux Type A-1 on Aluminum Bronze or Berryllium Copper) for good wetting. This alloy becomes extremely fluid above its melting point. With most joint designs a clearance of .001" to .003" (.025mm.-.075mm) is desirable.

Sil-Fos 18 should not be used on ferrous metals or nickel base alloys, since the phosphorus diffuses and produces brittle iron or nickel phosphides at the joint interface.

Information provided by Lucas-Milhaupt, Inc.

Available Properties
  • Specific Gravity
  • Density
  • Electrical Resistivity
  • Solidus
  • Liquidus
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。