Lucas-Milhaupt Lucanex 721 Active Metal Brazing
Subcategory: Silver Alloy; Copper Alloy; Indium Alloy; Nonferrous Metal; Solder/Braze Alloy
Close Analogs: Alloy compositions afer for filler metal powder in Lucanex paste
Material Notes: Brazing Paste Blended with Ti for active metal brazing of ceramics.Information provided by Lucas-Milhaupt, Inc.
| Available Properties |
- Particle Mesh Size
- Viscosity
- Solidus
- Liquidus
- Processing Temperature
- % Filler Metal Powder
- Color
|
|
|
|