Ametek Ultra 316L P/M Stainless Steel, Sintered from 6.49 g/cc Green Density
Subcategory: Stainless Steel; T 300 Series Stainless Steel; Metal
Key Words: Powder metallurgy
Material Notes: Iron content above calculated as balance. Ametek's patented Ultra Stainless Steels™ are produced by alloying the conventional austenitic compositions with a small amount of a copper-nickel-tin alloy. This results in a marked improvement in corrosion resistance, while other properties are comparable to the conventional counterparts. Mechanical property data below is from samples lubricated with 1% Acrawax C and pressed at 40 tsi. Green strength 1000 ksi. Specimens were delubricated in air for 20 min. at 950°F (510°C), then sintered in dissociated ammonia for 30 min. at 2100°F (1149°C) and cooled in the water jacketed furnace cooling zone. Dimensional change from die size -0.03%. Information provided by Ametek Specialty Metal Products.
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|