Ametek PF25 Nickel Alloy Thermal Spray Powder
Subcategory: Superalloy; Nickel Base
Key Words: Powder metallurgy
Material Notes: Nickel content above calculated as balance. Deposit has good machinability and impact resistance, slightly harder than PF20. Excellent corrosion resistance. May be used for repairs to cast iron parts or overlay where nickel base alloy is required. Ametek has developed this and other engineering alloys for hardfacing - the process of spraying and fusing metal powder onto a workpiece or substrate to give it specific hardness, wear, or corrosion resistant properties. Ametek® powders are engineered to have the precise size, spherical shape, and low oxygen content required for optimal thermal spraying characteristics. Information provided by Ametek Specialty Metal Products.
| Available Properties |
- Hardness, Rockwell C
- Melting Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|