Ametek High Purity Nickel Strip 899A Skin Hard
Subcategory: Nickel Alloy; Nonferrous Metal
Key Words: Nickel Alloy
Material Notes: Information supplied by Ametek Specialty Metal Products. AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including: - Lowest electrical resistivity available in pure nickel strip.
- Homogeneity, microcleanliness, and close composition control enhances weldability.
- Significantly low levels of surface oxides reduces die wear and provides excellent solderability.
- Excellent formability.
Typical applications for rechargeable batteries: computers, cellular phones, power tools, electric vehicles, pagers, and camcorders.
| Available Properties |
- Density
- Hardness, Rockwell B
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Poissons Ratio
- Electrical Resistivity
- Curie Temperature
- Thermal Conductivity
- Melting Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|