Meehanite Flake Graphite Type AQ Cast Iron
Subcategory: Gray Cast Iron; Metal
Material Notes: Type AQ is a wear and abrasion resisting iron that is readily machinable as-cast but may be "air-hardened" after machining with minimum risk of cracking or distortion. Type AQ is easily heat treated and locally hardened. Recommended for dies, punches, spinning mandrels and other hard wearing applications. General Meehanite information - Meehanite metal is first melted to a definite degree of undercooling or constitution which is related to the section of the casting to be poured and the range of physical properties such as tensile strength and hardness required. Nucleation with patented mixtures of graphitizing agents results in the removal of undercooling, in the controlled precipitation of graphite and in a fine grained eutectic cell structure which determines the density and physical integrity of the casting. Ordinary cast irons made to chemical specifications which do not include the benefit of controlled undercooling are influenced by mass effect to a maximum degree and for this and other reasons cannot be considered an equivalent to Meehanite metal. Information provided by Meehanite Marketing Association.
| Available Properties |
- Specific Gravity
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Modulus of Elasticity
- Modulus of Rupture
- Compressive Strength
- Poissons Ratio
- Izod Impact Unnotched
- Fatigue Strength
- Machinability
- Shear Modulus
- CTE, linear 68°F
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|