Meehanite Flake Graphite Type GM-60 Cast Iron
Subcategory: Gray Cast Iron; Metal
Material Notes: Type GM-60 possesses exceptionally high physical properties, including good impact strength and shock resistance. GM-60 responds well to heat treatment and surface hardening. Type GM machines to a very fine finish and is recommended for heavy section casting where pressure tightness is required. General Meehanite information - Meehanite metal is first melted to a definite degree of undercooling or constitution which is related to the section of the casting to be poured and the range of physical properties such as tensile strength and hardness required. Nucleation with patented mixtures of graphitizing agents results in the removal of undercooling, in the controlled precipitation of graphite and in a fine grained eutectic cell structure which determines the density and physical integrity of the casting. Ordinary cast irons made to chemical specifications which do not include the benefit of controlled undercooling are influenced by mass effect to a maximum degree and for this and other reasons cannot be considered an equivalent to Meehanite metal. Information provided by Meehanite Marketing Association.
| Available Properties |
- Specific Gravity
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Modulus of Elasticity
- Modulus of Rupture
- Compressive Strength
- Poissons Ratio
- Izod Impact Unnotched
- Fatigue Strength
- Machinability
- Shear Modulus
- Shear Strength
- CTE, linear 68°F
- Thermal Conductivity
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|