MetalTek MTEK 230 Aluminum Bronze
Subcategory: Copper Alloy; Aluminum Alloy; Nonferrous Metal; Bronze
Close Analogs: Cast UNS C95500; Cast Grade C95500; Cast ASTM B271, B505, B148
Key Words: Nickel Aluminum Bronze
Material Notes: Versatile alloy with high strength, good ductility, unusual toughness, plus exceptional wear resistance. Aluminum Bronze heat treated to higher mechanical properties where necessary.Information provided by MetalTek
| Available Properties |
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|