MetalTek MTEK 275 Aluminum Bronze
Subcategory: Copper Alloy; Aluminum Alloy; Nonferrous Metal; Bronze
Close Analogs: Cast UNS C95900; Cast Grade C95900; Cast ASTM B271, B505, B148
Material Notes: Engineered alloy for excellent wear and anti-galling properties in forming, bending and drawing dies. Aluminum Bronze heat treated to higher mechanical properties where necessary.Information provided by MetalTek
| Available Properties |
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|