MetalTek MTEK 375 Aluminum Bronze
Subcategory: Copper Alloy; Aluminum Alloy; Nonferrous Metal; Bronze
Material Notes: Engineered alloy for excellent wear and anti-galling properties in forming, bending and drawing dies. Aluminum Bronze heat treated to higher mechanical properties where necessary.Information provided by MetalTek
|
|
|