MetalTek MTEK 87-11-1-0-1 Gear Bronze
Subcategory: Copper Alloy; Tin Alloy; Nonferrous Metal; Bronze
Close Analogs: Cast UNS C92500; Cast Grade C92501; Cast ASTM B505
Key Words: Tin Bronze
Material Notes: Copper-tin alloy with high tensile, yield and compressive strength as well as wear resistance.Applications: Worm gears, steel mill nuts Information provided by MetalTek
| Available Properties |
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|