MetalTek MTEK 76-6-18 HI LEAD Bearing Bronze
Subcategory: Copper Alloy; Lead Alloy; Tin Alloy; Nonferrous Metal; Bronze
Close Analogs: Cast UNS C94100; Cast Grade C94100; Cast ASTM B66
Key Words: High Lead Tin Bronze
Material Notes: All popular tin/lead and high lead alloys with score resistance, structural uniformity, shear properties, compressive strength and low cost.Applications: Bearings, bushings, sleeves, liners, piston rings, hydraulic parts Information provided by MetalTek
| Available Properties |
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|
| Property Data |