MetalTek Bearium® B-8 Bearing Bronze
Subcategory: Copper Alloy; Lead Alloy; Nonferrous Metal; Bronze
Material Notes: Exceptional frictional properties as a result of uniformly dispersed microstructure constituents.Applications: Turbine thrust bearings, centrifuge bushings, shaft sleeves, and other severe duty, mission critical bearings and bushings. Information provided by MetalTek
| Available Properties |
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|