MetalTek Med. Tensile Manganese Bronze
Subcategory: Copper Alloy; Nonferrous Metal; Bronze
Close Analogs: Cast UNS C86200; Cast Grade C86200; Cast ASTM B271, B584, B148; Military MIL-C-15345-5; SAE 430A1
Key Words: Yellow Brass
Material Notes: High strength and hardness copper-zinc alloys, tensile strength up to 120,000 psi, (760 Mpa).Applications: Steel mill nuts, ordnance parts, worm gears. Information provided by MetalTek
| Available Properties |
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|