MetalTek Leaded Manganese Manganese Bronze
Subcategory: Copper Alloy; Nonferrous Metal; Bronze
Close Analogs: Cast UNS C86400; Cast Grade C86401; Cast ASTM B271, B584, B148
Key Words: Yellow Brass
Material Notes: High strength and hardness copper-zinc alloys, tensile strength up to 120,000 psi, (760 Mpa).Applications: Steel mill nuts, ordnance parts, worm gears. Information provided by MetalTek
| Available Properties |
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|