MetalTek NITRONIC® 60 Austenitic Stainless Steel
Subcategory: Stainless Steel; Metal; Austenitic
Close Analogs: Cast UNS J92972; Cast Grade CF10SMnN; Cast ASTM A351, A743; Wrought UNS S21800; Wrought Grade NITRONIC 60®
Material Notes: Wear and galling resistance. Produced under license of ARMCO Advanced Materials Corp. Applications: Pump wear rings, valve trim. Information provided by MetalTek
| Available Properties |
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Heat Treatment
|
|
|
|