MetalTek MTEK 20 Super Austenitic Stainless Steel
Subcategory: Stainless Steel; Metal; Austenitic
Close Analogs: Cast UNS N08007; Cast Grade CN7M; Cast ASTM A351, A743, A744; Wrought UNS N09020; Wrought Grade 20Cb-3®
Material Notes: Corrosion resistance approaching nickel alloys, especially in chloride service.Applications: Process piping exposed to flue gas and solutions. Information provided by MetalTek
| Available Properties |
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Heat Treatment
|
|
|
|