MetalTek 254 SMO® Super Austenitic Stainless Steel
Subcategory: Stainless Steel; Metal; Austenitic
Close Analogs: Cast UNS ; Cast Grade CK3MCuN; Cast ASTM A351, A743, A744; Wrought UNS S31254; Wrought Grade 254 SMO®
Material Notes: Corrosion resistance approaching nickel alloys, especially in chloride service. Produced under license of Avesta Jernverk AB. Applications: Process piping exposed to flue gas and solutions. Information provided by MetalTek
| Available Properties |
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Heat Treatment
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|