MetalTek MTEK 410 Martensitic Stainless Steel
Subcategory: T 400 Series Stainless Steel; Stainless Steel; T S40000 Series Stainless Steel; Metal; Martensitic
Close Analogs: Cast UNS J91150; Cast Grade CA15; Cast ASTM A743, A487; AMS 5351a; Wrought UNS S41000; Wrought Grade 410
Material Notes:
Information provided by MetalTek
| Available Properties |
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Heat Treatment
|
|
|
|