MetalTek MTEK 25-12 TYP I Heat Resistant Stainless Steel
Subcategory: Stainless Steel; Heat Resisting; Metal
Close Analogs: Cast UNS J93303; Cast Grade HH TYP I; Cast ASTM A447
Material Notes: Group of alloys very sensitive to composition balance. Suitable for a wide range of high temperature applications.Applications: Rable arms, radiant tubes, refractory support hardware, grate bars. Information provided by MetalTek
| Available Properties |
- Tensile Strength, Ultimate
- Elongation at Break
- Maximum Service Temperature, Air
- Heat Treatment
|
|
|
|