MetalTek MTEK 30-20 Heat Resistant Stainless Steel
Subcategory: Stainless Steel; Heat Resisting; Metal
Close Analogs: Cast UNS N08604; Cast Grade HL; Cast ASTM A297, A608
Material Notes: Provides strength levels of HK with improved corrosion resistance to hot gases.Applications: Similar to HN. Information provided by MetalTek
| Available Properties |
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Maximum Service Temperature, Air
- Heat Treatment
|
|
|
|