MetalTek MTEK A2 Tool Steel
Subcategory: Tool Steel; Metal
Close Analogs: Cast UNS T90102; Cast Grade CA2; Cast ASTM A597; Wrought UNS T30102; Wrought Grade AISI A2
Material Notes: Non-Deforming, wear/abrasion resistant.Applications: Forming rolls, dies, slitter blades. Information provided by MetalTek
| Available Properties |
- Hardness, Brinell
- Heat Treatment
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|