MetalTek HASTELLOY® S Severe Corrosion and Heat Resistant Alloy
Subcategory: Superalloy; Nickel Alloy; Heat Resisting
Close Analogs: Wrought UNS N06635; Wrought Grade HASTELLOY® S
Material Notes:
Information provided by MetalTek
| Available Properties |
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Heat Treatment
|
|
|
|
| Property Data |