Mi-Tech SW65, 35 Silver/65 Tungsten PM Metal Composite
Subcategory: Metal Matrix Composite; Silver Alloy; Tungsten Alloy; Nonferrous Metal
Key Words: Powder Metallurgy Metal Composite; Tungsten Alloys, Silver Alloys
Material Notes: Mi-Tech refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver. Silver-Tungsten is used when high oxidation-resistant materials are necessary and superior surface is required. Silver-tungsten is also widely used for tips on contact shoe facings used in high frequency continuous welding processes. Data provided by Mi-Tech Metals.
| Available Properties |
- Density
- Hardness, Rockwell B
- Electrical Resistivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|